| المادة | منخفض | مرتفع | الوحدة | الأساس |
|---|---|---|---|---|
| Graphite حرج Roughly 1 kg of anode material per kWh. | 50.00 | 80.00 | kg | Anode active material |
| Nickel حرج NMC811 cathode is roughly 0.7 kg Ni per kWh. | 40.00 | 60.00 | kg | Contained nickel |
| Aluminium حرج | 20.00 | 35.00 | kg | Cathode foil, cell cans and pack casing |
| Copper حرج | 15.00 | 25.00 | kg | Foil and busbars, cell and pack only |
| Cobalt حرج Falls sharply as cathodes move from NMC622 to NMC811. | 5.00 | 9.00 | kg | Contained cobalt |
| Lithium حرج About 0.10 kg Li per kWh of cell capacity. | 6.00 | 9.00 | kg contained lithium | Contained metal, not carbonate |
| Manganese حرج | 5.00 | 9.00 | kg | Contained manganese |
Indicative range compiled from published technology studies and chemistry; verify against a manufacturer specification before use. الصفوف المُوسَمة بـ«أثر» تحتوي على المادة بكميات صغيرة للغاية يتعذّر الإفصاح عنها بوصفها كتلة ذات دلالة — والقيد هنا يتعلق بالنقاء أو عدد الموردين، لا بالطنّاج.
البدائل
الإحلال هو القوة الأكثر استهانةً بها في عالم المواد. حين يغلو معدنٌ ما أو يصبح مثاراً للإشكاليات السياسية، يعمل المهندسون على تجاوزه في التصميم — وقد يتبخر الطلب على منجم بأكمله.

LFP Lithium-Ion Battery
Iron and phosphate instead of nickel and cobalt: heavier, cheaper, safer and very long-lived.

Sodium-Ion Battery
A cell that uses sodium — from ordinary salt — instead of lithium, at the cost of energy density.

Vanadium Redox Flow Battery
A battery that stores its energy in two tanks of dissolved vanadium, so power and capacity scale separately.